INFLUENCE OF SOLUTION TREATMENT TIME, ZN ADDITION AND COLD/HOT ROLLING ON THE MICROSTRUCTURE AND HARDNESS OF THE 2024 ALLOY

N/A
N/A
Protected

Academic year: 2020

Share "INFLUENCE OF SOLUTION TREATMENT TIME, ZN ADDITION AND COLD/HOT ROLLING ON THE MICROSTRUCTURE AND HARDNESS OF THE 2024 ALLOY"

Copied!
12
0
0

Texto completo

Loading

Figure

Fig. 1 SEM images (i) of 2024 alloy as a function of the Zn addition and solutilization time,  and elemental mapping (ii) of as-cast sample
Fig. 2 HV of 2024 alloy and of 2024 alloys with Zn additions solubilized for 3, 5 and 7h,  samples were 50 % hot working before solution treatment and after were 5 and 15% cold
Fig. 3 OM micrographs of 2024 alloy added with 0.5% wt. Zn after solubilized treatment for  3, 5 and in as-cast conditions, 50% hot rolling and 5 and 15% cold rolling
Fig. 4 HRB of 2024 alloy and of 2024 alloys with Zn additions after 5 % cold rolling and  reference sample as a function of aging time, solubilization time: a) 3h, b) 5h and c) 7h
+2

Referencias

Documento similar

In the Fornax cluster a larger fraction of galaxies tend to have lower SF activity, a smaller amount of atomic and molecular gas, and a higher SFE from the atomic or the total

Government policy varies between nations and this guidance sets out the need for balanced decision-making about ways of working, and the ongoing safety considerations

 The expansionary monetary policy measures have had a negative impact on net interest margins both via the reduction in interest rates and –less powerfully- the flattening of the

The c-BCN layer was found to be -25 nm thick and, therefore, the measure hardness is not reliable since the value is greatly influenced by the hardness of the thicker h-BCN

(hundreds of kHz). Resolution problems are directly related to the resulting accuracy of the computation, as it was seen in [18], so 32-bit floating point may not be appropriate

Citrus LHY gene LOC18047565 was down-regu- lated during the cold treatment period. However, its expression levels were always much higher in the CAR samples compared to the MAC

While the difference in hardness values of the W particles in both WNC and WNFC alloys is not significant, the matrix phase of WNC alloy is significantly harder in both heat

The Dwellers in the Garden of Allah 109... The Dwellers in the Garden of Allah